Verified by manufacturer 2 months ago
A single pack, vinyl sheen primer / finish. Offering adhesion to both clean steel, galvanized surfaces and existing prepared finishes such as Plastisol metal cladding.
Steel Fabrications
Once the surfaces to be coated are clean, dry and free from all contamination, grind down any sharp edges and shot blast to Sa2½ (as defined in ISO 8501-1) with an average surface profile of at least 50 microns. As an alternative to shot blasting, mechanically prepare the surfaces to St3-C or St3-D (as defined in ISO 8501-1). Painting should then be carried out within four hours.
When applied over freshly shotblasted steel a life expectancy to first maintenance of over 20 years is expected. For an ISO 12944 Class C2 environment a 120 micron dry film thickness over the peaks of shotblasted steel will offer a 15 year life to first maintenance, when applied in two airless spray coats.
Galvanized Steel
Ensure the surfaces to be coated are clean, dry and free from oily residues and other contaminates. New, bright, galvanised steel may be oiled or chemically treated, and this surface layer must be cleaned, degreased and tested by application of Mordant Solution to a small area. If the area of application turns entirely black, paint can be applied directly to the metal. If the colour change is uneven or fails to occur, degrease and repeat the test.
Plastisol Coating
Thoroughly wash and allow to dry. Remove any remaining contamination with a suitable degreaser and wipe with clean cloth or disposable paper towel. Localised repairs or damage should be lightly sanded to remove loose or flaky material until a sound edge is achieved. There is a tendency for the plasticisers in the Plastisol Coating to migrate in to the paint film and become tacky.
Plastisol cladding has a leatherette finish, a cladding with a smooth surface may be PDVF, PDVF cladding requires the use of a PDVF primer before application of Centrecoat cladding paint. For further details, please contact our technical department.
Centrecoat Cladding Protect Primer / Finish provides a flexible finish with high levels of impact resistance. It is suitable for refurbishing exterior metal cladding and particularly suitable for metal fabrications such as cladding, metal shutter doors, Plastisol cladding, glass, steel fabrications and more.
Also available in metallic shades.
With the ability to be applied in one single coat, this product is ideal when time constraints are demanding.
Color | Grey Yellow Green Blue Black |
Finish | Sheen |
Material | Vinyl Guidance for specification option: Vinyl Co-polymer. |
Shape | Formless |
Length | Bespoke |
Width | Bespoke |
Height | Bespoke |
Uniclass | |
CAWS | M60/195 Special coating M60/18 Special coating M60/175 Protective coating |
Composition | Vinyl co-polymer. |
Sheen | Low-sheen. |
Colour | 00-A-01.00-A-05.08-B-29.08-E-51.10-A-05.12-B-17.12-B-21.18-B-17.18-B-25.18-C-37.18-E-53.Black.Traffic Yellow (RAL 1023).Melon Yellow (RAL 1028).Pure Orange (RAL 2004).Traffic Red (RAL 3020).Signal Violet (RAL 4008).Signal Blue (RAL 5005).Blue Green (RAL 6004).Moss Green (RAL 6005).Pine Green (RAL 6028).Anthracite Grey (RAL 7016).White Aluminium (RAL 9006).Grey Aluminium (RAL 9007).Pure White (RAL 9010).White.Other.Guidance for specification option: Tintable in a wide range of colours including most British Standard and RAL shades. Consult manufacturer and insert requirements. Manufacturer guidanceConsult manufacturer for details. |
Viscosity | Thixotropic. |
Volume solids | 35–40%. Guidance for specification option: Depending on colour; consult manufacturer for details. |
VOC content | 588.0 g/L. |
Coverage | Approx. 5m²/L at 75 microns DFT. |
Wet film thickness (minimum) | 185 microns. |
Dry film thickness | 75 microns. |
Contains Red List materials | No |
Country of material origin | United Kingdom |
Country of product manufacture | United Kingdom |
Recyclability | Non Recyclable |
Recycled contentAs defined in clause 7.8 of BS EN ISO 14021 | 0 % |